Alodine treated HS-810 & HS-814
HS-810 and HS-814 after alodine treatment. My first attempt at Alodining was fruitless, wish I would of utilized the RV-List first. The instructions say to apply with a scotchbrite pad, don't waste your time again. Use the dip method, dip the part for 1 minute and rinse. The outcome is a nice golden color.
 